Mechanical Properties of Terbium and Plutonium

Add ⊕
1 Mechanical
1.1 Density
1.1.1 Density At Room Temperature
8.23 g/cm319.82 g/cm3
Mechanical Properties of Lithium
0.534 40.7
1.1.2 Density When Liquid (at m.p.)
7.65 g/cm316.63 g/cm3
Mechanical Properties of Lithium
0.512 20
1.2 Tensile Strength
60.00 MPaNA
Mechanical Properties of Indium
2.5 11000
1.3 Viscosity
NANA
Mechanical Properties of Mercury
0.001526 0.001526
1.4 Vapor Pressure
1.4.1 Vapor Pressure at 1000 K
0.00 (Pa)0.00 (Pa)
Mechanical Properties of Cerium
2.47E-11 121
1.4.2 Vapor Pressure at 2000 K
12.50 (Pa)2.20 (Pa)
Mechanical Properties of Tungsten
2.62E-10 774
1.5 Elasticity properties
1.5.1 Shear Modulus
22.10 GPa43.00 GPa
Mechanical Properties of Potassium
1.3 222
1.5.2 Bulk Modulus
38.70 GPaNA
Mechanical Properties of Cesium
1.6 462
1.5.3 Young's Modulus
55.70 GPa96.00 GPa
Mechanical Properties of Cesium
1.7 528
1.6 Poisson Ratio
0.260.21
Mechanical Properties of Beryllium
0.032 0.47
1.7 Other Mechanical Properties
Ductile, Malleable
Ductile, Malleable