8.23 g/cm3
7.65 g/cm3
60.00 MPa
0.00
0.00 (Pa)
12.50 (Pa)
22.10 GPa
38.70 GPa
55.70 GPa
0.26
Ductile, Malleable
 
19.10 g/cm3
17.30 g/cm3
100.00 MPa
0.00
0.00 (Pa)
0.01 (Pa)
111.00 GPa
100.00 GPa
208.00 GPa
0.23
Ductile, Malleable