Thermal Properties of Actinium and Platinum
Specific Heat
0.12 J/(kg K)
  
40
0.13 J/(kg K)
  
39
Molar Heat Capacity
27.20 J/mol·K
  
18
25.86 J/mol·K
  
35
Thermal Conductivity
12.00 W/m·K
  
99+
71.60 W/m·K
  
24
Critical Temperature
Not Available
  
Not Available
  
Thermal Expansion
Not Available
  
8.80 µm/(m·K)
  
99+
Enthalpy
  
  
Enthalpy of Vaporization
Not Available
  
510.50 kJ/mol
  
11
Enthalpy of Fusion
Not Available
  
19.70 kJ/mol
  
12
Enthalpy of Atomization
301.00 kJ/mol
  
36
565.00 kJ/mol
  
11
Standard Molar Entropy
56.50 J/mol.K
  
25
41.60 J/mol.K
  