Thermal Properties of Actinium and Uranium
Specific Heat
0.12 J/(kg K)
  
40
0.12 J/(kg K)
  
40
Molar Heat Capacity
27.20 J/mol·K
  
18
27.67 J/mol·K
  
15
Thermal Conductivity
12.00 W/m·K
  
99+
27.50 W/m·K
  
40
Critical Temperature
Not Available
  
Not Available
  
Thermal Expansion
Not Available
  
13.90 µm/(m·K)
  
27
Enthalpy
  
  
Enthalpy of Vaporization
Not Available
  
477.00 kJ/mol
  
13
Enthalpy of Fusion
Not Available
  
15.48 kJ/mol
  
19
Enthalpy of Atomization
301.00 kJ/mol
  
36
489.50 kJ/mol
  
14
Standard Molar Entropy
56.50 J/mol.K
  
25
50.20 J/mol.K
  