uranium
uranium

Lead
Lead



ADD
Compare
X
uranium
X
Lead

Teknik Properties saka uranium lan Lead

Add ⊕
Teknik

Kapadhetan Ing suhu kamar

Kapadhetan Nalika Liquid (ing mp)

Strength tensile

viskositas

Meksa beluk ing 1000 K

Meksa beluk ing 2000 K

nyukur pengaturan

pengaturan akeh

Young kang pengaturan

Poisson rasio

Properties Teknik liyane

 
12.45 g / cm 3
10.65 g / cm3
50.00 MPa
0.00
0.00 (Pa)
0.00 (Pa)
173.00 GPA
220.00 GPA
447.00 GPA
0.30
ductile, malleable
 
11.34 g / cm 3
10.66 g / cm3
12.00 MPa
0.00
1.64 (Pa)
0.00 (Pa)
5.60 GPA
46.00 GPA
16.00 GPA
0.44
ductile, malleable