Properties saka Beryllium lan Magnesium
leleh Point
1,278.00 ° C
  
36
650.00 ° C
  
99+
Boiling Point
2,970.00 ° C
  
32
1,107.00 ° C
  
99+
atose
  
  
Vickers atose
1,670.00 MPa
  
4
ora Sumadhiya
  
Properties Optical
  
  
bias Index
ora Sumadhiya
  
ora Sumadhiya
  
reflectivity
ora Sumadhiya
  
Kacepetan swara
12,890.00 m / s
  
2
4,940.00 m / s
  
11
allotropes
Ora
  
Ora
  
α allotropes
Ora Sumadhiya
  
Ora Sumadhiya
  
β allotropes
Ora Sumadhiya
  
Ora Sumadhiya
  
γ allotropes
Ora Sumadhiya
  
Ora Sumadhiya
  
Formula Kimia
Be
  
Mg
  
isotop
  
  
keelektronegatifan
  
  
Pauling Elektronegativitas
Sanderson Elektronegativitas
Allred Rochow Elektronegativitas
Mulliken-Jaffe Elektronegativitas
Electropositivity
  
  
Pauling Electropositivity
tenogo ionisasi
  
  
Level Energy 1st
899.50 kJ / mol
  
7
737.70 kJ / mol
  
24
Level Energy 2
1,757.10 kJ / mol
  
23
1,450.70 kJ / mol
  
99+
Level Energy 3rd
14,848.70 kJ / mol
  
2
7,732.70 kJ / mol
  
5
padha karo elektrokimia
0.17 g / amp-day
  
99+
0.45 g / amp-day
  
99+
Properties Kimia liyane
Corrosion, ionisasi, Isotop radioaktif
  
Corrosion, Highly Inflammable, ionisasi, kelarutan
  
Kapadhetan
  
  
Kapadhetan Ing suhu kamar
1.85 g / cm 3
  
99+
1.74 g / cm 3
  
99+
Kapadhetan Nalika Liquid (ing mp)
1.69 g / cm3
  
99+
1.58 g / cm3
  
99+
meksa beluk
  
  
Meksa beluk ing 1000 K
ora Sumadhiya
  
Meksa beluk ing 2000 K
ora Sumadhiya
  
ora Sumadhiya
  
Strength tensile
ora Sumadhiya
  
ora Sumadhiya
  
viskositas
ora Sumadhiya
  
ora Sumadhiya
  
situs kelenturan
  
  
Properties Teknik liyane
NA
  
NA
  
Symbol
Be
  
Mg
  
Panggil periode
2
  
3
  
Block
s pemblokiran
  
s pemblokiran
  
Family unsur
alkalin bumi
  
alkalin bumi
  
Volume atom
5.00 cm3 / mol
  
99+
13.97 cm3 / mol
  
37
Konfigurasi elektron
[Panjenenganipun] 2S 2
  
[Ne] 3s 2
  
Potensi Valence Electron
82.00 (-eV)
  
15
40.00 (-eV)
  
99+
atom
  
  
Struktur Crystal
Hexagonal Tutup dikempalken (HCP)
  
Hexagonal Tutup dikempalken (HCP)
  
Crystal pola
HCP-Crystal-Structure-of-Beryllium.jpg#100
  
HCP-Crystal-Structure-of-Magnesium.jpg#100
  
Radius saka Atom
  
  
pola Angles
π/2, π/2, π/2
  
π/2, π/2, 2 π/3
  
Pola C / A rasio
ora Sumadhiya
  
Nomer atom jejer
  
  
Properties Listrik
  
  
resistivity
36.00 nΩ · m
  
99+
43.90 nΩ · m
  
99+
konduktivitas listrik
0.31 10 6 / cm Ω
  
5
0.23 10 6 / cm Ω
  
7
elektron Affinity
0.00 kJ / mol
  
40
0.00 kJ / mol
  
40
Property Listrik
Semiconductor
  
Arman
  
Ciri Magnetic
  
  
Nindakake Magnetic
diamagnetic
  
paramagnetic
  
permeabilitas
ora Sumadhiya
  
ora Sumadhiya
  
kelemahan
ora Sumadhiya
  
ora Sumadhiya
  
Kalor tartamtu
1.82 J / (kg K)
  
2
1.02 J / (kg K)
  
4
doyo termal
200.00 W / m · K
  
6
156.00 W / m · K
  
8
suhu kritis
ora Sumadhiya
  
ora Sumadhiya
  
Graham Kapasitas kalor
16.44 J / mol · K
  
99+
24.87 J / mol · K
  
99+
Expansion termal
11.30 μm / (m · K)
  
34
24.80 μm / (m · K)
  
15
Standard molar Entropy
9.50 J / mol.K
  
99+
32.70 J / mol.K
  
99+
enthalpy
  
  
Enthalpy panguapan
294.70 kJ / mol
  
30
128.70 kJ / mol
  
99+
Enthalpy saka Fusion
11.72 kJ / mol
  
30
8.95 kJ / mol
  
39
Enthalpy saka atomization
326.40 kJ / mol
  
30
148.50 kJ / mol
  
99+