Tin
Mechanical Properties of Gadolinium and Tin


Mechanical Properties

Density
  
  

Density At Room Temperature
7.37 g/cm3   
99+
7.90 g/cm3   
99+

Density When Liquid (at m.p.)
6.99 g/cm3   
34
7.40 g/cm3   
31

Tensile Strength
Not Available   
Not Available   

Viscosity
Not Available   
Not Available   

Vapor Pressure
  
  

Vapor Pressure at 1000 K
0.00 (Pa)   
17
0.00 (Pa)   
30

Vapor Pressure at 2000 K
Not Available   
7.39 (Pa)   
9

Elasticity properties
  
  

Shear Modulus
18.00 GPa   
36
21.80 GPa   
33

Bulk Modulus
58.00 GPa   
20
37.90 GPa   
34

Young's Modulus
50.00 GPa   
36
54.80 GPa   
35

Poisson Ratio
0.36   
8
0.26   
23

Other Mechanical Properties
Ductile, Malleable   
Ductile, Malleable   

Magnetic >>
<< Atomic

Compare Post Transition Metals

Post-Transition Metals

Post-Transition Metals

» More Post-Transition Metals

Compare Post Transition Metals

» More Compare Post Transition Metals