Mechanical Properties of Praseodymium and Thulium


Mechanical Properties of Thulium and Praseodymium


Mechanical Properties

Density
  
  

Density At Room Temperature
6.77 g/cm3   
99+
9.32 g/cm3   
40

Density When Liquid (at m.p.)
6.50 g/cm3   
39
8.56 g/cm3   
24

Tensile Strength
Not Available   
Not Available   

Viscosity
Not Available   
Not Available   

Vapor Pressure
  
  

Vapor Pressure at 1000 K
0.00 (Pa)   
25
0.06 (Pa)   
10

Vapor Pressure at 2000 K
13.20 (Pa)   
7
Not Available   

Elasticity properties
  
  

Shear Modulus
14.80 GPa   
39
30.50 GPa   
22

Bulk Modulus
28.80 GPa   
40
44.50 GPa   
26

Young's Modulus
37.30 GPa   
99+
74.00 GPa   
27

Poisson Ratio
0.28   
16
0.21   
31

Other Mechanical Properties
Ductile, Malleable   
Ductile, Malleable   